| SCHEDA TECNICA SCHIUMA DI NEOPRENE | ||||||||||||
| TIPO |
DENSITÀ |
SPONDA C |
COMPRIMERE FORZA 25% |
CALORE RITIRO VALUTARE |
COMPRESSIONE SUL SET |
ACQUA ASSORBIMENTO |
TRAZIONE FORZA |
ALLUNGAMENTOTASSO DI |
SERVIZIO TEMP. |
MASSIMA DIMENSIONE |
||
| Kg/mq3 |
Grado |
Kpa |
(70 ℃ X4 ore) % |
(50%/72 cappello 23 ℃ ) |
% |
MPa |
% |
℃ |
mm |
|||
| ASTM D 1056 |
ASTM D 2240 |
ASTM D 1056 |
VDA753106 |
ASTM D 1056 |
ASTM D 1056 |
DIN53504 |
VDA 57310 |
|||||
| SCHIUMA SBR |
SBR9-11 |
130±20 |
9-11 | ≤5 |
≤2 |
≤25 |
≤3 | ≥0,8 |
≥220 |
-50~+130 |
30X1400X3400 |
|
| SBR 15-18 |
180±20 |
15-18 | ≤5 |
≤2 |
≤25 |
≤3 | ≥0,8 |
≥230 |
-50~+130 |
30X1400X3400 | ||
| SCHIUMA SCR | 15% CR 85% SBR |
180±20 | ≤5 | ≤2 | ≤25 | ≤3 | ≥0,8 | ≥230 | -50~+130 | 30X1400X3400 | ||
| 30% CR 70% SBR |
180±20 | ≤5 | ≤2 | ≤25 | ≤3 | ≥0,8 | ≥230 | -50~+130 | 30X1400X3400 | |||
| 50% CR 50% SBR |
180±20 | ≤5 | ≤2 | ≤25 | ≤3 | ≥0,8 | ≥230 | -50~+130 | 30X1400X3400 | |||
| SCHIUMA CR | 100% CR | 200±20 | ≤5 | ≤2 | ≤25 | ≤3 | ≥0,8 | ≥280 | -60~+180 | 30X1400X3400 | ||
| I DATI SOPRA SONO SOLO PER RIFERIMENTO, SOGGETTI AI PARAMETRI DEL PRODOTTO DELL'ORDINE EFFETTIVO | ||||||||||||